{"operation":"document","citation":"49 CFR 178.364-4","title":"Tests.","source_type":"regulation","agency":"Pipeline and Hazardous Materials Safety Administration","status":"historical","official":true,"published_on":null,"effective_on":"2003-10-01","summary":"Prior to each use, each overpack must be visually inspected for defects such as wood checking or splintering weld cracking, corrosion of steel parts, improper joint bonding, or improperly fitting closure lid.\n\n[Amdt. 178-35, 39 FR 45253, Dec. 31, 1974. Redesigntated by Amdt. 178-97, 55 FR 52716, Dec","machine_formats":{"json":"https://regulus.evalyn.ai/document/49-cfr-178-364-4.json","markdown":"https://regulus.evalyn.ai/document/49-cfr-178-364-4.md"},"app_url":"https://regulus.evalyn.ai/document/49-cfr-178-364-4","source_url":"https://www.govinfo.gov/app/details/CFR-2003-title49-vol2/CFR-2003-title49-vol2-sec178-364-4","body":"Prior to each use, each overpack must be visually inspected for defects such as wood checking or splintering weld cracking, corrosion of steel parts, improper joint bonding, or improperly fitting closure lid.\n\n[Amdt. 178-35, 39 FR 45253, Dec. 31, 1974. Redesigntated by Amdt. 178-97, 55 FR 52716, Dec. 21, 1990; 66 FR 45389, Aug. 28, 2001]","truncated":false,"body_characters":339}