# -5 Postweld heat treatment and corrosion resistance.

- **operation:** document
- **citation:** 49 CFR 179.201-5
- **title:** -5 Postweld heat treatment and corrosion resistance.
- **source type:** regulation
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** current
- **official:** true
- **published on:** Not available
- **effective on:** 2026-08-18
- **summary:** (a) Tanks and attachments welded directly thereto must be postweld heat treated as a unit at the proper temperature except as indicated below. Tanks and attachments welded directly thereto fabricated from ASTM A 240/A 240M (IBR, see § 171.7 of this subchapter) Type 430A, Type 304 and Type 316 materi
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/49-cfr-179-201-5.json
- **markdown:** https://regulus.evalyn.ai/document/49-cfr-179-201-5.md
- **app url:** https://regulus.evalyn.ai/document/49-cfr-179-201-5
- **source url:** https://www.ecfr.gov/on/2026-08-18/title-49/section-179.201-5
**body:**

(a) Tanks and attachments welded directly thereto must be postweld heat treated as a unit at the proper temperature except as indicated below. Tanks and attachments welded directly thereto fabricated from ASTM A 240/A 240M (IBR, see § 171.7 of this subchapter) Type 430A, Type 304 and Type 316 materials must be postweld heat treated as a unit and must be tested to demonstrate that they possess the corrosion resistance specified in § 179.200-7(d), Footnote 2. Tanks and attachments welded directly thereto, fabricated from ASTM A 240/A 240M Type 304L or Type 316L materials are not required to be postweld heat treated.

(b) Tanks and attachments welded directly thereto, fabricated from ASTM A 240/A 240M Type 304L and Type 316 materials must be tested to demonstrate that they possess the corrosion resistance specified in § 179.200-7(d), Footnote 2.

[68 FR 75762, Dec. 31, 2003]