# Wrinkle bends in steel pipe.

- **operation:** document
- **citation:** 49 CFR 192.315
- **title:** Wrinkle bends in steel pipe.
- **source type:** regulation
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** current
- **official:** true
- **published on:** Not available
- **effective on:** 2026-08-18
- **summary:** (a) A wrinkle bend may not be made on steel pipe to be operated at a pressure that produces a hoop stress of 30 percent, or more, of SMYS.

(b) Each wrinkle bend on steel pipe must comply with the following:

(1) The bend must not have any sharp kinks.

(2) When measured along the crotch of the bend
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/49-cfr-192-315.json
- **markdown:** https://regulus.evalyn.ai/document/49-cfr-192-315.md
- **app url:** https://regulus.evalyn.ai/document/49-cfr-192-315
- **source url:** https://www.ecfr.gov/on/2026-08-18/title-49/section-192.315
**body:**

(a) A wrinkle bend may not be made on steel pipe to be operated at a pressure that produces a hoop stress of 30 percent, or more, of SMYS.

(b) Each wrinkle bend on steel pipe must comply with the following:

(1) The bend must not have any sharp kinks.

(2) When measured along the crotch of the bend, the wrinkles must be a distance of at least one pipe diameter.

(3) On pipe 16 inches (406 millimeters) or larger in diameter, the bend may not have a deflection of more than 1 1/2° for each wrinkle.

(4) On pipe containing a longitudinal weld the longitudinal seam must be as near as practicable to the neutral axis of the bend.

[35 FR 13257, Aug. 19, 1970, as amended by Amdt. 192-85, 63 FR 37503, July 13, 1998]