- **summary:** § 192.309 Repair of Steel Pipe (a) Each imperfection or damage that impairs the serviceability of a length of steel pipe must be repaired or removed. If a repair is made by grinding, the remaining wall thickness must at least be equal to either: (1) The minimum thickness required by the tolerances i
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/ar-car-23-500-192-309.json
- **markdown:** https://regulus.evalyn.ai/document/ar-car-23-500-192-309.md
- **app url:** https://regulus.evalyn.ai/document/ar-car-23-500-192-309
- **source url:** https://codeofarrules.arkansas.gov/Rules/Rule?chapterID=40&levelType=part&partID=1394&subChapterID=392&titleID=23
**body:**

§ 192.309 Repair of Steel Pipe (a) Each imperfection or damage that impairs the serviceability of a length of steel pipe must be repaired or removed. If a repair is made by grinding, the remaining wall thickness must at least be equal to either: (1) The minimum thickness required by the tolerances in the specification to which the pipe was manufactured; or (2) The nominal wall thickness required for the design pressure of the pipeline. (b) Each of the following dents must be removed from steel pipe to be operated at a pressure that produces a hoop stress of 20 percent, or more, of SMYS, unless the dent is repaired by a method that reliable engineering tests and analyses show can permanently restore the serviceability of the pipe: (1) A dent that contains a stress concentrator such as a scratch, gouge, groove, or arc burn. (2) A dent that affects the longitudinal weld or a circumferential weld. (3) In pipe to be operated at a pressure that produces a hoop stress of 40 percent or more of SMYS, a dent that has a depth of: (i) More than 1/4 inch (6.4 millimeters) in pipe 12 3/4 inches (324 millimeters) or less in outer diameter; or (ii) More than 2 percent of the nominal pipe diameter in pipe over 12 3/4 inches (324 millimeters) in outer diameter. For the purpose of this section a "dent" is a depression that produces a gross disturbance in the curvature of the pipe wall without reducing the pipe-wall thickness. The depth of a dent is measured as the gap between the lowest point of the dent and a prolongation of the original contour of the pipe. (c) Each arc burn on steel pipe to be operated at a pressure that produces a hoop stress of 40 percent, or more, of SMYS must be repaired or removed. If a repair is made by grinding, the arc burn must be completely removed and the remaining wall thickness must be at least equal to either: (1) The minimum wall thickness required by the tolerances in the specification to which the pipe was manufactured; or (2) The nominal wall thickness required for the design pressure of the pipeline. (d) A gouge, groove, arc burn, or dent may not be repaired by insert patching or by pounding out. (e) Each gouge, groove, arc burn, or dent that is removed from a length of pipe must be removed by cutting out the damaged portion as a cylinder.