# Remedial Measures: Cast Iron and Ductile Iron Pipelines [49 CFR 192.489]

- **operation:** document
- **citation:** LAC 43:XIII §2141
- **title:** Remedial Measures: Cast Iron and Ductile Iron Pipelines [49 CFR 192.489]
- **source type:** regulation
- **agency:** Louisiana Office of Conservation
- **status:** current
- **official:** true
- **published on:** Not available
- **effective on:** Not available
- **summary:** A. General Graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced. [49 CFR 192.489(a)] B. Localized Graphitization. Each segment of cast iron or ductile iron pipe on which loca
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/la-lac-43-xiii-2141.json
- **markdown:** https://regulus.evalyn.ai/document/la-lac-43-xiii-2141.md
- **app url:** https://regulus.evalyn.ai/document/la-lac-43-xiii-2141
- **source url:** https://www.doa.la.gov/doa/osr/louisiana-administrative-code/
**body:**

A. General Graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced. [49 CFR 192.489(a)]

B. Localized Graphitization. Each segment of cast iron or ductile iron pipe on which localized graphitization is found to a degree where any leakage might result, must be replaced or repaired, or sealed by internal sealing methods adequate to prevent or arrest any leakage. [49 CFR 192.489(b)]

AUTHORITY NOTE: Promulgated in accordance with R.S. 30:501 et seq.

HISTORICAL NOTE: Promulgated by the Department of Natural Resources, Office of Conservation, LR 9:237 (April 1983), amended LR 10:529 (July 1984), LR 30:1256 (June 2004).
- **truncated:** false