# PHMSA Hazmat Incident E-2008080341 — OXIDIZING SOLID, CORROSIVE, N.O.S. — DETROIT, MI

- **operation:** document
- **citation:** PHMSA Hazmat Incident E-2008080341
- **title:** PHMSA Hazmat Incident E-2008080341 — OXIDIZING SOLID, CORROSIVE, N.O.S. — DETROIT, MI
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2008-08-01
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2008-08-01 in DETROIT, MI.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2008080341.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2008080341.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2008080341
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=m5RkxPFtYzG%2BHhaSxa9WHQ%3D%3D
**body:**

PHMSA hazardous materials incident report E-2008080341.
Incident date: 2008-08-01.
Location: DETROIT, MI.
Mode: Highway.
Carrier/reporter: Nortru, LLC.
Shipper: Valspar.
Materials: UN3085; OXIDIZING SOLID, CORROSIVE, N.O.S.; hazard class 5.1; 3724 SLB released.
What failed: Inner Packaging.
How failed: Burst or Ruptured.
Reported failure causes: Commodity Self-Ignition.
Reported result: Fire.
Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.