# PHMSA Hazmat Incident E-2012080443 — PHOSPHORIC ACID SOLUTION — SPRING, TX

- **operation:** document
- **citation:** PHMSA Hazmat Incident E-2012080443
- **title:** PHMSA Hazmat Incident E-2012080443 — PHOSPHORIC ACID SOLUTION — SPRING, TX
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2012-08-11
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2012-08-11 in SPRING, TX.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2012080443.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2012080443.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2012080443
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=6vrPDrRcJqnGqULuXNe8Ww%3D%3D
**body:**

PHMSA hazardous materials incident report E-2012080443.
Incident date: 2012-08-11.
Location: SPRING, TX.
Mode: Rail.
Carrier/reporter: PCS NITROGEN FERTILIZER OPERATIONS, INC..
Shipper: PCS Phosphate Inc..
Materials: UN1805; PHOSPHORIC ACID SOLUTION; hazard class 8; 5499.25 LGA released.
What failed: Liner.
How failed: Leaked.
Reported failure causes: Defective Component or Device.
Reported result: Spillage.