# PHMSA Hazmat Incident E-2015040377 — RESIN SOLUTION, FLAMMABLE — CHEROKEE, AL

- **operation:** document
- **citation:** PHMSA Hazmat Incident E-2015040377
- **title:** PHMSA Hazmat Incident E-2015040377 — RESIN SOLUTION, FLAMMABLE — CHEROKEE, AL
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2015-03-25
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2015-03-25 in CHEROKEE, AL.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2015040377.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2015040377.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-e-2015040377
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=Nci3BQfiOLD4ghmolVacnQ%3D%3D
**body:**

PHMSA hazardous materials incident report E-2015040377.
Incident date: 2015-03-25.
Location: CHEROKEE, AL.
Mode: Highway.
Carrier/reporter: R&L Carriers.
Shipper: AOC, LLC / Ashland Chemical / Bio-Cide International / RAPAC, L.P..
Materials: UN1866; RESIN SOLUTION, FLAMMABLE; hazard class 3; 750 LGA released | UN1908; CHLORITE SOLUTION; hazard class 8; 64.125 LGA released | UN2211; POLYMERIC BEADS, EXPANDABLE, EVOLVING FLAMMABLE VAPOR; hazard class 9; 4800 SLB released | UN3266; CORROSIVE LIQUID, BASIC, INORGANIC, N.O.S.; hazard class 8; 103.125 LGA released.
What failed: Body.
How failed: Burst or Ruptured.
Reported failure causes: Fire, Temperature, or Heat.
Reported result: Fire.
Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.
- **truncated:** false