# PHMSA Hazmat Incident I-1981040202 — VINYL ACETATE, STABILIZED — DAYTON, NJ

- **operation:** document
- **citation:** PHMSA Hazmat Incident I-1981040202
- **title:** PHMSA Hazmat Incident I-1981040202 — VINYL ACETATE, STABILIZED — DAYTON, NJ
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 1981-04-15
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 1981-04-15 in DAYTON, NJ.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1981040202.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1981040202.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1981040202
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=P1Dp3CyqS2B8bjToQ%2FurVg%3D%3D
**body:**

PHMSA hazardous materials incident report I-1981040202.
Incident date: 1981-04-15.
Location: DAYTON, NJ.
Mode: Highway.
Carrier/reporter: HETEM BROS INC.
Shipper: CELENESE CHEM.
Materials: UN1301; VINYL ACETATE, STABILIZED; hazard class 3; 7000 LGA released.
How failed: Punctured.
Reported failure causes: Rollover Accident; Vehicular Crash or Accident Damage.
Reported result: Spillage.
Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.