# PHMSA Hazmat Incident I-1998051376 — PHOSPHORIC ACID SOLUTION — HOWE, IN

- **operation:** document
- **citation:** PHMSA Hazmat Incident I-1998051376
- **title:** PHMSA Hazmat Incident I-1998051376 — PHOSPHORIC ACID SOLUTION — HOWE, IN
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 1998-05-12
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 1998-05-12 in HOWE, IN.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1998051376.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1998051376.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-1998051376
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=kw3R7HTQQgZ%2FzpuJSr04%2Bg%3D%3D
**body:**

PHMSA hazardous materials incident report I-1998051376.
Incident date: 1998-05-12.
Location: HOWE, IN.
Mode: Highway.
Carrier/reporter: WASTE MANAGEMENT OF OHIO.
Shipper: ABLE ELECTRO POLISHING CO.
Materials: UN1805; PHOSPHORIC ACID SOLUTION; hazard class 8; 500 LGA released.
Reported failure causes: Fire, Temperature, or Heat; Incompatible Product.
Reported result: Spillage, Material Entered Waterway/Storm Sewer, Environmental Damage.