# PHMSA Hazmat Incident I-2001060923 — SULFUR, MOLTEN — BEAUMONT, TX

- **operation:** document
- **citation:** PHMSA Hazmat Incident I-2001060923
- **title:** PHMSA Hazmat Incident I-2001060923 — SULFUR, MOLTEN — BEAUMONT, TX
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2001-05-20
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2001-05-20 in BEAUMONT, TX.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2001060923.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2001060923.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2001060923
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=jPLAnO%2FFTeQVgFa97tUq5w%3D%3D
**body:**

PHMSA hazardous materials incident report I-2001060923.
Incident date: 2001-05-20.
Location: BEAUMONT, TX.
Mode: Highway.
Carrier/reporter: MARTIN TRANSPORT CO INC.
Shipper: MOBIL OIL CORP.
Materials: NA2448; SULFUR, MOLTEN; hazard class 9; 200 LGA released.
What failed: Basic Material.
Reported failure causes: Vehicular Crash or Accident Damage.
Reported result: Spillage.