# PHMSA Hazmat Incident I-2007080748 — PHOSPHORIC ACID SOLUTION — MEMPHIS, TN

- **operation:** document
- **citation:** PHMSA Hazmat Incident I-2007080748
- **title:** PHMSA Hazmat Incident I-2007080748 — PHOSPHORIC ACID SOLUTION — MEMPHIS, TN
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2007-08-10
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2007-08-10 in MEMPHIS, TN.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2007080748.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2007080748.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2007080748
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=9bS0D0u%2F6cVE4PQfHnQ9wg%3D%3D
**body:**

PHMSA hazardous materials incident report I-2007080748.
Incident date: 2007-08-10.
Location: MEMPHIS, TN.
Mode: Air.
Carrier/reporter: FEDERAL EXPRESS CORPORATION.
Shipper: MAGCHEM INC..
Materials: UN1805; PHOSPHORIC ACID SOLUTION; hazard class 8; 0.063401 LGA released.
What failed: Weld or Seam.
How failed: Punctured.
Reported failure causes: Impact with Sharp or Protruding Object (e.g., nails).
Reported result: Spillage.
Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.