# PHMSA Hazmat Incident I-2020040227 — SULFURIC ACID WITH NOT MORE THAN 51% ACID — AUSTIN, AR

- **operation:** document
- **citation:** PHMSA Hazmat Incident I-2020040227
- **title:** PHMSA Hazmat Incident I-2020040227 — SULFURIC ACID WITH NOT MORE THAN 51% ACID — AUSTIN, AR
- **source type:** incident
- **agency:** Pipeline and Hazardous Materials Safety Administration
- **status:** historical
- **official:** true
- **published on:** Not available
- **effective on:** 2020-02-25
- **summary:** Serious reporter-submitted hazardous materials transportation incident on 2020-02-25 in AUSTIN, AR.
- **machine formats:** - **json:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2020040227.json
- **markdown:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2020040227.md
- **app url:** https://regulus.evalyn.ai/document/phmsa-hazmat-incident-i-2020040227
- **source url:** https://portal.phmsa.dot.gov/PDFGenerator/getPublicReport/OHMIR_5800-1-PUBLIC?INCIDENTID=%2FVJZgRalCyfdyF%2BqHNdCfw%3D%3D
**body:**

PHMSA hazardous materials incident report I-2020040227.
Incident date: 2020-02-25.
Location: AUSTIN, AR.
Mode: Highway.
Carrier/reporter: LEGACY REGIONAL TRANSPORT, LLC.
Shipper: FUTUREFUEL CHEMICAL COMPANY.
Materials: UN2796; SULFURIC ACID WITH NOT MORE THAN 51% ACID; hazard class 8; 5607.5 LGA released.
Reported result: Spillage.
Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.
- **truncated:** false