PHMSA Hazmat Incident E-2012050453
PHMSA Hazmat Incident E-2012050453
Incident E-2012050453PHMSA hazardous materials incident report E-2012050453. Incident date: 2012-05-12. Location: LINCOLN, NE. Mode: Highway. Carrier/reporter: Southern Refrigerated Transport. Shipper: Akzo Nobol Surface Chemistry, LLC. Materials: UN3267; CORROSIVE LIQUID, BASIC, ORGANIC, N.O.S.; hazard class 8; 75 LGA released. What failed: Body. How failed: Cracked. Reported failure causes: Inadequate Blocking and Bracing. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#
This material provides agency context. It does not replace binding regulatory text, and its legal effect depends on the underlying authority and facts.