PHMSA Hazmat Incident I-1979061810
PHMSA Hazmat Incident I-1979061810
Incident I-1979061810PHMSA hazardous materials incident report I-1979061810. Incident date: 1979-05-05. Location: LINCOLN, NE. Mode: Rail. Carrier/reporter: BURLINGTON NORTHERN INC. Shipper: TEXAS GULF INC. Materials: UN1805; PHOSPHORIC ACID SOLUTION; hazard class 8; 31500 SLB released. Reported failure causes: Corrosion - Exterior. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#
This material provides agency context. It does not replace binding regulatory text, and its legal effect depends on the underlying authority and facts.