PHMSA Hazmat Incident I-1984090136
PHMSA Hazmat Incident I-1984090136
Incident I-1984090136PHMSA hazardous materials incident report I-1984090136. Incident date: 1984-08-31. Location: BROWNWOOD, TX. Mode: Rail. Carrier/reporter: ATCHISON TOPEKA & SANTA FE RY. Shipper: KENNECOTT COPPER CORP. Materials: UN1830; SULFURIC ACID; hazard class 8; 250 LGA released. What failed: Auxiliary Valve; Basic Material; Bottom Outlet Valve; Piping or Fittings. Reported failure causes: Defective Component or Device. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#
This material provides agency context. It does not replace binding regulatory text, and its legal effect depends on the underlying authority and facts.