Incident I-1990050592PHMSA hazardous materials incident report I-1990050592. Incident date: 1989-12-05. Location: HOUSTON, TX. Mode: Highway. Carrier/reporter: AM-PET SERV INC. Shipper: AM-PET SERV INC. Materials: UN1824; SODIUM HYDROXIDE, SOLUTION; hazard class 8; 293.75 LGA released. What failed: Liner; Weld or Seam; Weld or Seam. How failed: Burst or Ruptured; Punctured; Ripped or Torn; Burst or Ruptured; Punctured; Ripped or Torn. Reported failure causes: Corrosion - Exterior; Dropped; Dropped; Corrosion - Exterior. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#