PHMSA Hazmat Incident I-2003091094
PHMSA Hazmat Incident I-2003091094
Incident I-2003091094PHMSA hazardous materials incident report I-2003091094. Incident date: 2003-08-25. Location: LINKWOOD, MD. Mode: Highway. Carrier/reporter: LIQUID TRANSPORTERS INC. Shipper: GULBRANDSEN MFG INC. Materials: UN2582; FERRIC CHLORIDE, SOLUTION; hazard class 8; 1800 LGA released. What failed: Auxiliary Valve; Piping or Fittings. Reported failure causes: Corrosion - Exterior; Incompatible Product. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#
This material provides agency context. It does not replace binding regulatory text, and its legal effect depends on the underlying authority and facts.