Incident I-2005010056PHMSA hazardous materials incident report I-2005010056. Incident date: 2004-12-07. Location: BROADUS, MT. Mode: Highway. Carrier/reporter: LYNDEN TRANSPORT INC. Shipper: CRITERION CATALYSTS & TECH. Materials: UN3190; SELF-HEATING SOLID, INORGANIC, N.O.S.; hazard class 4.2; 1500 SLB released. What failed: Basic Material. How failed: Punctured; Cracked; Crushed. Reported failure causes: Vehicular Crash or Accident Damage. Reported result: Spillage. Reporter-submitted DOT Form 5800.1 data may be incomplete, corrected, supplemented, or misreported. A record, serious-incident classification, failure description, or relationship to a reporting rule is not a PHMSA causal finding, compliance determination, or finding of a violation.#